Print Back
Cold Rolled, Annealed No. 2B Finish
Can also be furnished:
No. 3 Finish - Polished One or Two Sides
No. 4 Finish - Polished One or Two Sides
Non-Magnetic (May be Slightly magnetic when cold worked)
Paper Interleaved or Vinyl Masked:
22 Gauge and Heavier
A.S.T.M. A480/A240 ASME SA-240
A.S.T.M. A262 Prac E
Unit of Measure

Specifications

Material

N/A Type 317L Stainless Steel

Shapeform

N/A Coil

Thickness

N/A 19 gauge

Thickness

N/A 0.042 inches1.0668 mm

Size

N/A 48 x Coil

Width

N/A 48

Sheet Weight per Unit Area

N/A 1.764 lbs/ft²8.611848 kg/m²

Finish

N/A No. 2B No. 3 No. 4

Condition

N/A Cold Rolled Annealed

Nominal Composition

N/A 0.08% Max. Carbon 1.00% Max. Silicon 11.00 to 15.00% Nickel 18.00 to 20.00% Chrominum 2.0 to 3.0% Molybdenum 2.00% Max. Manganese

ASTM Specification

N/A ASTM A240 ASTM A262 Prac E ASTM A480 ASTM SA-240 UNS S31700

Typical Mechanical Properties

Steel Alloy Group

N/A Austenitic

Magnetic Properties

N/A Non-Magnetic

Harden By

N/A Cold Work

Corrosion Resistance

N/A High

Hardness

N/A Low to Med.

Strength

N/A Low to Med.

Ductility

N/A High

Toughness

N/A High

Elec. Conductance

N/A Low

Thermal Conductance

N/A Low

Thermal Expansion

N/A High

Heat Resistance (Scaling Strength)

N/A High/High

Comparative Characteristics and Applications

Density

N/A 0.29 lbs/in³

Modulus of Elasticity in Tension

N/A 28.0 x 106 lbs/in²

Specific Heat (32 to 212°F)

N/A 0.12 BTU/ºF/lbs

Thermal Conductivity at 212°F

N/A 9.4 BTU/hr.ft²/ft/ºF

Thermal Conductivity at 932°F

N/A 12.4 BTU/hr.ft²/ft/ºF

Mean Coefficient of Thermal Expansion per °F (32 to 212°F)

N/A 8.9 x 10-6 ºF

Mean Coefficient of Thermal Expansion per °F (32 to 600°F)

N/A 9.0 x 10-6 ºF

Mean Coefficient of Thermal Expansion per °F (32 to 1000°F)

N/A 9.7 x 10-6 ºF

Mean Coefficient of Thermal Expansion per °F (32 to 1200°F)

N/A 10.3 x 10-6 ºF

Melting Point Range

N/A 2500 to 2550 ºF

Electrical Resistivity

N/A 74 µΩ.cm

Max. Operating Temp. (Continuous Service)

N/A 1700 ºF

Max. Operating Temp. (Intermittent Service)

N/A 1600 ºF

Welding Properties

N/A Very Good-Tough Welds

Drawing and Stamping

N/A Good

Hot Working - Initial Forging

N/A 2100 to 2300 ºF

Annealing Temp.

N/A 1850 to 2050 ºF

Stress Relieving Temp.

N/A 400 to 750 ºF

Applications

N/A

  • Rapid transit cars, buses, aircraft, cargo containers
  • Retractor springs
  • Hose clamps
  • Conveyors
  • Bottling machinery
  • Jewelry
  • Cryogenic vessels and components
  • Still tubes
  • Expand metal parts
  • Mixing bowls
  • Dryers
  • Furnace parts
  • Heat exchangers
  • Paper mill equipment
  • Oil refining equipment
  • Textile industry
  • Dyeing equipment
  • Jet engine parts
  • Welded storage tanks for organic chemicals
  • Combustion chambers
  • Furnace arch supports
  • Kiln linings
  • Smoke control ductwork
  • Coal chutes
  • Gauge parts
  • Cutlery
  • Fish hooks
  • Glass molds
  • Bank vaults
  • Fasteners
  • Skewers
  • Dairy industry
  • Burner and emission control components
  • Recuperators
  • Pipes, tubes