Material |
N/A Type 301 Stainless Steel |
Shapeform |
N/A Coil & Strip |
Thickness |
N/A 0.035 inches0.8890 mm |
Maximum Coil Width |
N/A 24 inches |
Strip Weight per Unit Area |
N/A 1.4616 lbs/ft²7.1355312 kg/m² |
Weight |
N/A 2.9232 lbs/ft4.35030624 kg/m |
Temper |
N/A Hard |
Nominal Composition |
N/A 0.03% Max. Sulphur 0.045% Max. Phosphorus 0.10% Nitrogen 0.15% Max. Carbon 1.00% Max. Silicon 16.00 to 18.00% Chrominum 2.00% Max. Manganese 6.00 to 8.00% Nickel |
ASTM Specification |
N/A ASTM A240 ASTM A262 Prac E ASTM A480 ASTM A666 UNS S30100 |
Steel Alloy Group |
N/A Austenitic |
Magnetic Properties |
N/A Non-Magnetic |
Harden By |
N/A Cold Work |
Corrosion Resistance |
N/A High |
Hardness |
N/A Low to Med. |
Strength |
N/A Low to Med. |
Ductility |
N/A High |
Toughness |
N/A High |
Elec. Conductance |
N/A Low |
Thermal Conductance |
N/A Low |
Thermal Expansion |
N/A High |
Heat Resistance (Scaling Strength) |
N/A High/High |
Yield Strength |
N/A 140000 lbs/in² |
Tensile Strength |
N/A 185000 lbs/in² |
Elongation percent in 2 inches |
N/A 9 % |
Hardness (Rockwell B) |
N/A 40 |
Density |
N/A 0.29 lbs/in³ |
Modulus of Elasticity in Tension |
N/A 28.0 x 106 lbs/in² |
Specific Heat (32 to 212°F) |
N/A 0.12 BTU/ºF/lbs |
Thermal Conductivity at 212°F |
N/A 9.4 BTU/hr.ft²/ft/ºF |
Thermal Conductivity at 932°F |
N/A 12.4 BTU/hr.ft²/ft/ºF |
Mean Coefficient of Thermal Expansion per °F (32 to 212°F) |
N/A 9.4 x 10-6 ºF |
Mean Coefficient of Thermal Expansion per °F (32 to 600°F) |
N/A 9.5 x 10-6 ºF |
Mean Coefficient of Thermal Expansion per °F (32 to 1000°F) |
N/A 10.1 x 10-6 ºF |
Mean Coefficient of Thermal Expansion per °F (32 to 1200°F) |
N/A 10.4 x 10-6 ºF |
Melting Point Range |
N/A 2550 to 2590 ºF |
Electrical Resistivity |
N/A 69 µΩ.cm |
Max. Operating Temp. (Continuous Service) |
N/A 1600 ºF |
Max. Operating Temp. (Intermittent Service) |
N/A 1500 ºF |
Welding Properties |
N/A Very Good-Tough Welds |
Drawing and Stamping |
N/A Good |
Hot Working - Initial Forging |
N/A 2100 to 2300 ºF |
Annealing Temp. |
N/A 1850 to 2050 ºF |
Stress Relieving Temp. |
N/A 400 to 750 ºF |
Applications |
N/A Has mechanical properties desired for spring S. Good fatigue life. |