Items |
409-26-36-C Stainless Steel Sheet and Coil - Type 409 |
409-24-36-C Stainless Steel Sheet and Coil - Type 409 |
409-24-48-C Stainless Steel Sheet and Coil - Type 409 |
409-22-36-C Stainless Steel Sheet and Coil - Type 409 |
409-22-48-C Stainless Steel Sheet and Coil - Type 409 |
|||||
Material | N/A Type 409 Stainless Steel | |||||||||
Shapeform | N/A Coil | |||||||||
Preparation | N/A Paper Interleaved | |||||||||
Thickness | N/A 26 gauge | N/A 24 gauge | N/A 24 gauge | N/A 22 gauge | N/A 22 gauge | |||||
Thickness | N/A 0.018 inches0.4572 mm | N/A 0.024 inches0.6096 mm | N/A 0.024 inches0.6096 mm | N/A 0.030 inches0.762 mm | N/A 0.030 inches0.762 mm | |||||
Size | N/A 36 x Coil | N/A 36 x Coil | N/A 48 x Coil | N/A 36 x Coil | N/A 48 x Coil | |||||
Width | N/A 36 | N/A 36 | N/A 48 | N/A 36 | N/A 48 | |||||
Length | N/A | |||||||||
Sheet Weight per Unit Area | N/A 0.742 lbs/ft²3.622444 kg/m² | N/A 0.989 lbs/ft²4.828298 kg/m² | N/A 0.989 lbs/ft²4.828298 kg/m² | N/A 1.236 lbs/ft²6.034152 kg/m² | N/A 1.236 lbs/ft²6.034152 kg/m² | |||||
Estimated Weight per Sheet | N/A | |||||||||
Finish | N/A No. 2D | |||||||||
Condition | N/A Cold Rolled Annealed | |||||||||
Nominal Composition | N/A 0 or trace Nickel 0.06 to 0.35% Carbon 0.75% Max. Titanium x Carbon Min 1.00% Max. Manganese 1.00% Max. Silicon 10.50 to 11.75% Chrominum | |||||||||
ASTM Specification | N/A ASTM A240 ASTM A480 ASTM SA-240 UNS N40900 | |||||||||
Steel Alloy Group | N/A Ferritic | |||||||||
Magnetic Properties | N/A Magnetic | |||||||||
Harden By | N/A Cold Work | |||||||||
Corrosion Resistance | N/A Med. to High | |||||||||
Hardness | N/A Low | |||||||||
Strength | N/A Low | |||||||||
Ductility | N/A Med. | |||||||||
Toughness | N/A Low to Med. | |||||||||
Elec. Conductance | N/A Med. | |||||||||
Thermal Conductance | N/A Med. | |||||||||
Thermal Expansion | N/A Med. | |||||||||
Heat Resistance (Scaling Strength) | N/A High/Low | |||||||||
Yield Strength | N/A 35000 lbs/in² | |||||||||
Tensile Strength | N/A 62000 lbs/in² | |||||||||
Elongation percent in 2 inches | N/A 68 % | |||||||||
Hardness (Rockwell B) | N/A 68 | |||||||||
Density | N/A 0.28 lbs/in³ | |||||||||
Modulus of Elasticity in Tension | N/A 29.0 x 106 lbs/in² | |||||||||
Specific Heat (32 to 212°F) | N/A 0.11 BTU/ºF/lbs | |||||||||
Thermal Conductivity at 212°F | N/A 14.4 BTU/hr.ft²/ft/ºF | |||||||||
Mean Coefficient of Thermal Expansion per °F (32 to 212°F) | N/A 6.5 x 10-6 ºF | |||||||||
Mean Coefficient of Thermal Expansion per °F (32 to 1200°F) | N/A 7.2 x 10-6 ºF | |||||||||
Melting Point Range | N/A 2600 to 2750 ºF | |||||||||
Electrical Resistivity | N/A 60 µΩ.cm | |||||||||
Max. Operating Temp. (Continuous Service) | N/A 1250 ºF | |||||||||
Max. Operating Temp. (Intermittent Service) | N/A 1400 ºF | |||||||||
Welding Properties | N/A Good Fairly-Tough Welds | |||||||||
Drawing and Stamping | N/A Good | |||||||||
Hot Working - Initial Forging | N/A 1900 to 2100 ºF | |||||||||
Annealing Temp. | N/A 1500 to 1800 ºF | |||||||||