Print Back
10' - 14' Random Lengths
Annealed and Pickled
A.S.T.M. A276

Standard sizes also available in low carbon grade (304-L)
Also available as slit or sheared edge conditioned bar (1/8"-1/2").
Unit of Measure

Specifications

Material

N/A Type 316 Stainless Steel

Shapeform

N/A Rectangular Bar

Thickness x Width

N/A 1/8 x 5/8 inches

Working Decimal Equivalent

N/A 0.125 x 0.625 inches3.175 x 15.875 mm

Thickness

N/A 1/8 inches

Width

N/A 5/8 inches

Weight

N/A 0.2657 lbs/ft0.3953616 kg/m

Weight per 12' Length

N/A 3.188 lbs1.444164 kg

Finish

N/A No. 2B

Condition

N/A Annealed Pickled

Nominal Composition

N/A 0 to 0.25% Carbon 1.00% Max. Silicon 2.00% Max. Manganese 6 to 36% Nickel 7 to 30% Chrome

ASTM Specification

N/A ASTM A276 UNS S31600

Random Length

N/A 10 to 14

Typical Mechanical Properties

Steel Alloy Group

N/A Austenitic

Magnetic Properties

N/A Non-Magnetic

Harden By

N/A Cold Work

Corrosion Resistance

N/A High

Hardness

N/A Low to Med.

Strength

N/A Low to Med.

Ductility

N/A High

Toughness

N/A High

Elec. Conductance

N/A Low

Thermal Conductance

N/A Low

Thermal Expansion

N/A High

Heat Resistance (Scaling Strength)

N/A High/High

Comparative Characteristics and Applications

Yield Strength

N/A 45000 lbs/in²

Tensile Strength

N/A 18200 lbs/in²

Elongation percent in 2 inches

N/A 50 %

Hardness (Rockwell B)

N/A 83

Creep Strength Load for 10000 Hr. with 1% Elongation at 1000°F

N/A 25000 lbs/in²

Creep Strength Load for 10000 Hr. with 1% Elongation at 1100°F

N/A 18200 lbs/in²

Creep Strength Load for 10000 Hr. with 1% Elongation at 1200°F

N/A 12700 lbs/in²

Creep Strength Load for 10000 Hr. with 1% Elongation at 1300°F

N/A 7900 lbs/in²

Density

N/A 0.29 lbs/in³

Modulus of Elasticity in Tension

N/A 29.0 x 106 lbs/in²

Specific Heat (32 to 212°F)

N/A 0.12 BTU/ºF/lbs

Thermal Conductivity at 212°F

N/A 9.4 BTU/hr.ft²/ft/ºF

Thermal Conductivity at 932°F

N/A 12.4 BTU/hr.ft²/ft/ºF

Mean Coefficient of Thermal Expansion per °F (32 to 212°F)

N/A 8.8 x 10-6 ºF

Mean Coefficient of Thermal Expansion per °F (32 to 600°F)

N/A 9.0 x 10-6 ºF

Mean Coefficient of Thermal Expansion per °F (32 to 1000°F)

N/A 9.7 x 10-6 ºF

Mean Coefficient of Thermal Expansion per °F (32 to 1200°F)

N/A 10.3 x 10-6 ºF

Melting Point Range

N/A 2500 to 2550 ºF

Electrical Resistivity

N/A 74 µΩ.cm

Max. Operating Temp. (Continuous Service)

N/A 1650 ºF

Max. Operating Temp. (Intermittent Service)

N/A 1500 ºF

Welding Properties

N/A Very Good-Tough Welds

Drawing and Stamping

N/A Good

Hot Working - Initial Forging

N/A 2100 to 2300 ºF

Annealing Temp.

N/A 1850 to 2050 ºF

Stress Relieving Temp.

N/A 400 to 750 ºF

Applications

N/A

  • Rapid transit cars, buses, aircraft, cargo containers
  • Retractor springs
  • Hose clamps
  • Conveyors
  • Bottling machinery
  • Jewelry
  • Cryogenic vessels and components
  • Still tubes
  • Expand metal parts
  • Mixing bowls
  • Dryers
  • Furnace parts
  • Heat exchangers
  • Paper mill equipment
  • Oil refining equipment
  • Textile industry
  • Dyeing equipment
  • Jet engine parts
  • Welded storage tanks for organic chemicals
  • Combustion chambers
  • Furnace arch supports
  • Kiln linings
  • Smoke control ductwork
  • Coal chutes
  • Gauge parts
  • Cutlery
  • Fish hooks
  • Glass molds
  • Bank vaults
  • Fasteners
  • Skewers
  • Dairy industry
  • Burner and emission control components
  • Recuperators
  • Pipes, tubes