Hot Rolled, Annealed and Pickled
20' Random Lengths A.S.T.M. A276
Most sizes also available in low carbon grade (304L, 316L)
20' Random Lengths A.S.T.M. A276
Most sizes also available in low carbon grade (304L, 316L)
Unit of Measure
Specifications
|
Typical Mechanical Properties
|
Comparative Characteristics and Applications
|
Applications
Specifications
Material |
N/A Type 304 Stainless Steel |
Shapeform |
N/A Angle |
Size |
N/A 2 x 2 x 1/8 inches |
Working Decimal Equivalent |
N/A 2.000 x 2.000 x 0.125 inches50.8 x 50.8 x 3.175 mm |
Height |
N/A 2 inches |
Width |
N/A 2 inches |
Length |
N/A 1/8 inches |
Weight |
N/A 1.6473 lbs/ft2.4511824 kg/m |
Weight per 20' Length |
N/A 32.945 lbs14.924085 kg |
Finish |
N/A No. 2B |
Condition |
N/A Hot Rolled Annealed Pickled |
Nominal Composition |
N/A 0 to 0.25% Carbon 1.00% Max. Silicon 2.00% Max. Manganese 6 to 36% Nickel 7 to 30% Chrome |
ASTM Specification |
N/A ASTM A276 UNS S30400 |
Random Length |
N/A 10 to 14 |
Typical Mechanical Properties
Steel Alloy Group |
N/A Austenitic |
Magnetic Properties |
N/A Non-Magnetic |
Harden By |
N/A Cold Work |
Corrosion Resistance |
N/A High |
Hardness |
N/A Low to Med. |
Strength |
N/A Low to Med. |
Ductility |
N/A High |
Toughness |
N/A High |
Elec. Conductance |
N/A Low |
Thermal Conductance |
N/A Low |
Thermal Expansion |
N/A High |
Heat Resistance (Scaling Strength) |
N/A High/High |
Comparative Characteristics and Applications
Yield Strength |
N/A 46000 lbs/in² |
Tensile Strength |
N/A 89000 lbs/in² |
Elongation percent in 2 inches |
N/A 55 % |
Hardness (Rockwell B) |
N/A 86 |
Creep Strength Load for 10000 Hr. with 1% Elongation at 1000°F |
N/A 17000 lbs/in² |
Creep Strength Load for 10000 Hr. with 1% Elongation at 1100°F |
N/A 12000 lbs/in² |
Creep Strength Load for 10000 Hr. with 1% Elongation at 1200°F |
N/A 7000 lbs/in² |
Creep Strength Load for 10000 Hr. with 1% Elongation at 1300°F |
N/A 4000 lbs/in² |
Density |
N/A 0.29 lbs/in³ |
Modulus of Elasticity in Tension |
N/A 28.0 x 106 lbs/in² |
Specific Heat (32 to 212°F) |
N/A 0.12 BTU/ºF/lbs |
Thermal Conductivity at 212°F |
N/A 9.4 BTU/hr.ft²/ft/ºF |
Thermal Conductivity at 932°F |
N/A 12.4 BTU/hr.ft²/ft/ºF |
Mean Coefficient of Thermal Expansion per °F (32 to 212°F) |
N/A 9.6 x 10-6 ºF |
Mean Coefficient of Thermal Expansion per °F (32 to 600°F) |
N/A 9.9 x 10-6 ºF |
Mean Coefficient of Thermal Expansion per °F (32 to 1000°F) |
N/A 10.2 x 10-6 ºF |
Mean Coefficient of Thermal Expansion per °F (32 to 1200°F) |
N/A 10.4 x 10-6 ºF |
Melting Point Range |
N/A 2550 to 2650 ºF |
Electrical Resistivity |
N/A 72 µΩ.cm |
Max. Operating Temp. (Continuous Service) |
N/A 1650 ºF |
Max. Operating Temp. (Intermittent Service) |
N/A 1500 ºF |
Welding Properties |
N/A Very Good-Tough Welds |
Drawing and Stamping |
N/A Very Good |
Hot Working - Initial Forging |
N/A 2100 to 2300 ºF |
Annealing Temp. |
N/A 1850 to 2050 ºF |
Stress Relieving Temp. |
N/A 400 to 750 ºF |
Applications
N/A
|