Stainless Steel Plate - Type 410S
Stainless Steel Plate
Hot Rolled, Annealed and Pickled
A.S.T.M. A240/A480 ASME SA-240
Unit of Measure
Items |
/Asset/Titanium-Plate.jpg 410S-1875-48-96 Stainless Steel Plate - Type 410S |
/Asset/Titanium-Plate.jpg 410S-1875-48-120 Stainless Steel Plate - Type 410S |
/Asset/Titanium-Plate.jpg 410S-1875-48-144 Stainless Steel Plate - Type 410S |
/Asset/Titanium-Plate.jpg 410S-1875-48-240 Stainless Steel Plate - Type 410S |
/Asset/Titanium-Plate.jpg 410S-1875-96-240 Stainless Steel Plate - Type 410S |
|||||
Material | N/A Type 410S Stainless Steel | |||||||||
Shapeform | N/A Plates | |||||||||
Thickness | N/A 3/16 inches | |||||||||
Thickness | N/A 0.1875 inches4.7625 mm | |||||||||
Size | N/A 48 x 96 inches | N/A 48 x 120 inches | N/A 48 x 144 inches | N/A 48 x 240 inches | N/A 96 x 240 inches | |||||
Width | N/A 48 inches | N/A 48 inches | N/A 48 inches | N/A 48 inches | N/A 96 inches | |||||
Length | N/A 96 inches | N/A 120 inches | N/A 144 inches | N/A 240 inches | N/A 240 inches | |||||
Plate Weight per Unit Area | N/A 8.579 lbs/ft²41.882678 kg/m² | N/A | N/A | N/A | N/A | |||||
Weight per Plate | N/A 275 lbs124.73791 kg | N/A 343 lbs155.5821932 kg | N/A 412 lbs186.8800688 kg | N/A 686 lbs311.1643864 kg | N/A 1373 lbs622.7823652 kg | |||||
Finish | N/A No. 2B | |||||||||
Condition | N/A Hot Rolled Annealed Pickled | |||||||||
Nominal Composition | N/A 0 or trace Nickel 0.06 to 0.35% Carbon 0.75% Max. Titanium x Carbon Min 1.00% Max. Manganese 1.00% Max. Silicon 10.50 to 11.75% Chrominum | |||||||||
ASTM Specification | N/A ASME SA-240 ASTM A240 ASTM A480 UNS S41008 | |||||||||
Steel Alloy Group |
N/A Ferritic | |||||||||
Magnetic Properties | N/A Magnetic | |||||||||
Harden By | N/A Cold Work | |||||||||
Corrosion Resistance | N/A Med. to High | |||||||||
Hardness | N/A Low | |||||||||
Strength | N/A Low | |||||||||
Ductility | N/A Med. | |||||||||
Toughness | N/A Low to Med. | |||||||||
Elec. Conductance | N/A Med. | |||||||||
Thermal Conductance | N/A Med. | |||||||||
Thermal Expansion | N/A Med. | |||||||||
Heat Resistance (Scaling Strength) | N/A High/Low | |||||||||
Yield Strength | N/A 49000 lbs/in² | |||||||||
Tensile Strength | N/A 70000 lbs/in² | |||||||||
Elongation percent in 2 inches | N/A 31 % | |||||||||
Hardness (Rockwell B) | N/A 85 | |||||||||
Creep Strength Load for 10000 Hr. with 1% Elongation at 1000°F | N/A 9000 lbs/in² | |||||||||
Creep Strength Load for 10000 Hr. with 1% Elongation at 1100°F | N/A 4200 lbs/in² | |||||||||
Creep Strength Load for 10000 Hr. with 1% Elongation at 1200°F | N/A 4000 lbs/in² | |||||||||
Creep Strength Load for 10000 Hr. with 1% Elongation at 1300°F | N/A 1000 lbs/in² | |||||||||
Density | N/A 0.28 lbs/in³ | |||||||||
Modulus of Elasticity in Tension | N/A 29.0 x 106 lbs/in² | |||||||||
Specific Heat (32 to 212°F) | N/A 0.11 BTU/ºF/lbs | |||||||||
Thermal Conductivity at 212°F | N/A 14.4 BTU/hr.ft²/ft/ºF | |||||||||
Thermal Conductivity at 932°F | N/A 16.6 BTU/hr.ft²/ft/ºF | |||||||||
Mean Coefficient of Thermal Expansion per °F (32 to 212°F) | N/A 9.3 x 10-6 ºF | |||||||||
Mean Coefficient of Thermal Expansion per °F (32 to 600°F) | N/A 9.5 x 10-6 ºF | |||||||||
Mean Coefficient of Thermal Expansion per °F (32 to 1000°F) | N/A 10.3 x 10-6 ºF | |||||||||
Mean Coefficient of Thermal Expansion per °F (32 to 1200°F) | N/A 10.7 x 10-6 ºF | |||||||||
Melting Point Range | N/A 2700 to 2750 ºF | |||||||||
Electrical Resistivity | N/A 57 µΩ.cm | |||||||||
Max. Operating Temp. (Continuous Service) | N/A 1250 ºF | |||||||||
Max. Operating Temp. (Intermittent Service) | N/A 1400 ºF | |||||||||
Welding Properties | N/A Fair-Preheat 400-500°F, Anneal 1250°F after welding | |||||||||
Drawing and Stamping | N/A Fair-Good | |||||||||
Hot Working - Initial Forging | N/A 2000 to 2200 ºF | |||||||||
Annealing Temp. | N/A 1500 to 1650 ºF | |||||||||
Applications |
N/A
|
|||||||||
|