Stainless Steel Pipe -Type 316L Schedule 40S
Stainless Steel Pipes
Seamless and Welded
Full Finished, Annealed, Pickled
20' Random Lengths A.S.T.M. A312
Full Finished, Annealed, Pickled
20' Random Lengths A.S.T.M. A312
Unit of Measure
Items |
/Asset/Stainless-Pipe2.jpg 316L-125-405-40S Stainless Steel Pipe -Type 316L Schedule 40S |
/Asset/Stainless-Pipe2.jpg 316L-250-540-40S Stainless Steel Pipe -Type 316L Schedule 40S |
/Asset/Stainless-Pipe2.jpg 316L-375-675-40S Stainless Steel Pipe -Type 316L Schedule 40S |
/Asset/Stainless-Pipe2.jpg 316L-500-840-40S Stainless Steel Pipe -Type 316L Schedule 40S |
/Asset/Stainless-Pipe2.jpg 316L-750-1050-40S Stainless Steel Pipe -Type 316L Schedule 40S |
|||||
Material | N/A Type 316L Stainless Steel | |||||||||
Shapeform | N/A Pipe | |||||||||
Nominal I.P.S. | N/A 1/8 inches | N/A 1/4 inches | N/A 3/8 inches | N/A 1/2 inches | N/A 3/4 inches | |||||
O.D. | N/A 0.405 inches10.287 mm | N/A 0.54 inches13.716 mm | N/A 0.675 inches17.145 mm | N/A 0.84 inches21.336 mm | N/A 1.05 inches26.67 mm | |||||
Wall Thickness | N/A 0.068 inches1.7272 mm | N/A 0.088 inches2.2352 mm | N/A 0.091 inches2.3114 mm | N/A 0.109 inches2.7686 mm | N/A 0.113 inches2.8702 mm | |||||
Weight | N/A 0.245 lbs/ft0.36460018 kg/m | N/A 0.425 lbs/ft0.6324697 kg/m | N/A 0.568 lbs/ft0.845277152 kg/m | N/A 0.851 lbs/ft1.266427564 kg/m | N/A 1.131 lbs/ft1.683113484 kg/m | |||||
Standard | N/A Schedule 40S | |||||||||
Condition | N/A Fully Finished Annealed Pickled | |||||||||
Nominal Composition | N/A 0 to 0.25% Carbon 1.00% Max. Silicon 2.00% Max. Manganese 6 to 36% Nickel 7 to 30% Chrome | |||||||||
ASTM Specification | N/A ASTM A312 UNS S31603 | |||||||||
Random Length | N/A 20 ft | |||||||||
Steel Alloy Group |
N/A Austenitic | |||||||||
Magnetic Properties | N/A Non-Magnetic | |||||||||
Harden By | N/A Cold Work | |||||||||
Corrosion Resistance | N/A High | |||||||||
Hardness | N/A Low to Med. | |||||||||
Strength | N/A Low to Med. | |||||||||
Ductility | N/A High | |||||||||
Toughness | N/A High | |||||||||
Elec. Conductance | N/A Low | |||||||||
Thermal Conductance | N/A Low | |||||||||
Thermal Expansion | N/A High | |||||||||
Heat Resistance (Scaling Strength) | N/A High/High | |||||||||
Yield Strength | N/A 45000 lbs/in² | |||||||||
Tensile Strength | N/A 18200 lbs/in² | |||||||||
Elongation percent in 2 inches | N/A 50 % | |||||||||
Hardness (Rockwell B) | N/A 83 | |||||||||
Creep Strength Load for 10000 Hr. with 1% Elongation at 1000°F | N/A 25000 lbs/in² | |||||||||
Creep Strength Load for 10000 Hr. with 1% Elongation at 1100°F | N/A 7900 lbs/in² | |||||||||
Creep Strength Load for 10000 Hr. with 1% Elongation at 1200°F | N/A 7900 lbs/in² | |||||||||
Creep Strength Load for 10000 Hr. with 1% Elongation at 1300°F | N/A 7900 lbs/in² | |||||||||
Density | N/A 0.29 lbs/in³ | |||||||||
Modulus of Elasticity in Tension | N/A 29.0 x 106 lbs/in² | |||||||||
Specific Heat (32 to 212°F) | N/A 0.12 BTU/ºF/lbs | |||||||||
Thermal Conductivity at 212°F | N/A 9.04 BTU/hr.ft²/ft/ºF | |||||||||
Thermal Conductivity at 932°F | N/A 12.4 BTU/hr.ft²/ft/ºF | |||||||||
Mean Coefficient of Thermal Expansion per °F (32 to 212°F) | N/A 8.9 x 10-6 ºF | |||||||||
Mean Coefficient of Thermal Expansion per °F (32 to 600°F) | N/A 9.0 x 10-6 ºF | |||||||||
Mean Coefficient of Thermal Expansion per °F (32 to 1000°F) | N/A 9.7 x 10-6 ºF | |||||||||
Mean Coefficient of Thermal Expansion per °F (32 to 1200°F) | N/A 10.3 x 10-6 ºF | |||||||||
Melting Point Range | N/A 2500 to 2550 ºF | |||||||||
Electrical Resistivity | N/A 74 µΩ.cm | |||||||||
Max. Operating Temp. (Continuous Service) | N/A 1700 ºF | |||||||||
Max. Operating Temp. (Intermittent Service) | N/A 1600 ºF | |||||||||
Welding Properties | N/A Good | |||||||||
Drawing and Stamping | N/A Good | |||||||||
Hot Working - Initial Forging | N/A 2100 to 2300 ºF | |||||||||
Annealing Temp. | N/A 1950 to 2050 ºF | |||||||||
Stress Relieving Temp. | N/A 400 to 750 ºF | |||||||||