Inconel® C-276 is a nickel-molybdenum-chromium alloy with an addition of tungsten, having excellent corrosion resistance in a wide range of severe environments. The high molybdenum content makes the alloy especially resistant to pitting and crevice corrosion. The low carbon content minimizes carbide precipitation during welding to maintain corrosion resistance in as-welded structures. Inconel C-276 used in pollution control, chemical processing, pulp and paper production, and waste treatment. Standard product forms are round, forging stock, pipe, tube, plate, sheet, strip and wire.
Unit of Measure
Items
Nickel and High Temperature Alloy Plate

Inconel® C-276 Plate

Nickel and High Temperature Alloy Plate

Inconel® C-276 Plate

Nickel and High Temperature Alloy Plate

Inconel® C-276 Plate

Nickel and High Temperature Alloy Plate

Inconel® C-276 Plate

Nickel and High Temperature Alloy Plate

Inconel® C-276 Plate
Material N/A Inconel®
Shapeform N/A Plates
Thickness N/A 3/16 inches N/A 1/4 inches N/A 3/8 inches N/A 1/2 inches N/A 5/8 inches
Thickness N/A 0.1875 inches4.75 mm N/A 0.25 inches6.3500 mm N/A 0.375 inches9.52 mm N/A 0.500 inches12.7 mm N/A 0.625 inches15.87 mm
Plate Weight per Unit Area N/A 0.0639 lbs/in²44.92614744 kg/m² N/A 0.0855 lbs/in²60.1124508 kg/m² N/A 0.127 lbs/in²89.2898392 kg/m² N/A 0.17 lbs/in²119.521832 kg/m² N/A 0.206 lbs/in²144.8323376 kg/m²
Alloy N/A Inconel® C-276
Basic Composition N/A 1.1% Silicon 15.5% Chrominum 16.0% Molybdenum 57.0% Nickel
Density N/A 0.321 lbs/in³8.89 g/cm³
ASTM Specification N/A ASME SB-575 ASTM B575 UNS N010276
Melting Temperature Range N/A 2415 to 2500 ºF1325 to 1370 ºC
Tensile Strength N/A 115000 psi790 MPa
Yield Strength (0.2% Offset) N/A 60000 psi415 MPa
Elongation N/A 50 %