Incoloy® 800HT Plate
Incoloy®
Incoloy 800HT is a nickel-iron-chromium alloy with good strength and excellent resistance to oxidation and carburization in high-temperature atmospheres. It also resists corrosion by many aqueous environments. Incoloy 800HT maintains a stable, austenitic structure during prolonged exposure to high temperatures.
Incoloy 800HT is used for process piping, heat exchangers, carburizing equipment, heating-element sheathing and nuclear steam-generator tubing. Standard product forms are round, flats, forging stock, pipe, tube, plate, sheet, strip and wire.
Unit of Measure
Items |
/Asset/nickel-plate.jpg I800HT-1875 Incoloy® 800HT Plate |
/Asset/nickel-plate.jpg I800HT-250 Incoloy® 800HT Plate |
/Asset/nickel-plate.jpg I800HT-3125 Incoloy® 800HT Plate |
/Asset/nickel-plate.jpg I800HT-375 Incoloy® 800HT Plate |
/Asset/nickel-plate.jpg I800HT-500 Incoloy® 800HT Plate |
|||||
Material | N/A Incoloy® | |||||||||
Shapeform | N/A Plates | |||||||||
Thickness | N/A 3/16 inches | N/A 1/4 inches | N/A 5/16 inches | N/A 3/8 inches | N/A 1/2 inches | |||||
Thickness | N/A 0.1875 inches4.75 mm | N/A 0.25 inches6.3500 mm | N/A 0.3125 inches7.92 mm | N/A 0.375 inches9.52 mm | N/A 0.500 inches12.7 mm | |||||
Plate Weight per Unit Area | N/A 0.06000 lbs/in²42.184176 kg/m² | N/A 0.07900 lbs/in²55.5424984 kg/m² | N/A 0.09700 lbs/in²68.1977512 kg/m² | N/A 0.1169 lbs/in²82.18883624 kg/m² | N/A 0.15350 lbs/in²107.9211836 kg/m² | |||||
Alloy | N/A Incoloy 800HT | |||||||||
Basic Composition | N/A 0.015% Max. Sulphur 0.10% Carbon 0.60% Aluminum 0.60% Titanium 0.75% Max. Copper 1.0% Max. Silicon 1.20% Aluminum +Titanium 1.50% Max. Manganese 23.0% Chrominum 35.0% Nickel 39.5% Min. Iron | |||||||||
Density | N/A 0.287 lbs/in³7.94 g/cm³ | |||||||||
ASTM Specification | N/A ASME SB-409 ASTM B409 UNS N08811 | |||||||||
Melting Temperature Range | N/A 2475 to 2525 ºF1357 to 1385 ºC | |||||||||
Rupture Strength (1000 h at 1200°F/650°C) | N/A 24000 psi165 MPa | |||||||||
Rupture Strength (1000 h at 1300°F/705°C) | N/A 15000 psi105 MPa | |||||||||
Rupture Strength (1000 h at 1400°F/760°C) | N/A 10000 psi70 MPa | |||||||||
Rupture Strength (1000 h at 1600°F/870°C) | N/A 4700 psi32 MPa | |||||||||
Rupture Strength (1000 h at 1800°F/980°C) | N/A 2000 psi14 MPa | |||||||||
|